# Build Plate Idea - Pure Garolite

**URL:** <https://forum.lulzbot.com/t/build-plate-idea-pure-garolite/21301>\
**Category:** Community\
**Created:** [April 11, 2020, 1:37am UTC](https://forum.lulzbot.com/t/build-plate-idea-pure-garolite/21301 "2020-04-11T01:37:17Z")\
**Posts on this page:** 2\
**Page:** 1

<div class="post-metadata">

**Author:** ![jallen14108](https://sea2.discourse-cdn.com/flex020/user_avatar/forum.lulzbot.com/jallen14108/32/10412_2.png) [@jallen14108](https://forum.lulzbot.com/u/jallen14108)\
**Post date:** [April 11, 2020, 1:37am UTC](https://forum.lulzbot.com/t/build-plate-idea-pure-garolite/21301/1 "2020-04-11T01:37:17Z")

</div>

I print on a machined garolite plate. The garolite is exactly the size of the modular glass plate including thickness. It is a direct replacement for the glass plate. I use it for my nylon prints and I use magigoo PA or some PVA stick. I think it may be better for other materials that don’t work with glass very well. (PETG destroyed my last glass plate…) Or perhaps I am just saving my glass for my PLA prints…

Some of you new Lulzbot guys in Fargo might consider this a product idea. I would love to buy them than hire a machine shop to make them for me.

---

<div class="post-metadata">

**Author:** ![jallen14108](https://sea2.discourse-cdn.com/flex020/user_avatar/forum.lulzbot.com/jallen14108/32/10412_2.png) [@jallen14108](https://forum.lulzbot.com/u/jallen14108)\
**Post date:** [April 11, 2020, 1:43am UTC](https://forum.lulzbot.com/t/build-plate-idea-pure-garolite/21301/2 "2020-04-11T01:43:02Z")

</div>

Just a note: I sand the garolite on the print side to make a rough surface for the PVA to bind to. The heat side is marked in marker as “heater side”. Its just too smooth to be a good print surface. Its the main advantage over glass.