Infill to perimeter issues

I was never too consumed with my Taz print quality until recently. I’ve been dialing in several materials to get the best results for a while now. I noticed that when my printer moves from the infill to the perimeter on a test cube that it jerks very quickly during that step and makes ridges every so many layers on the corners of cubes. You can see it more on the left side of this image. It’s pretty pronounced. This was sliced in S3D. I’m about to run a test in Cura to see if it does the same. Has anyone seen this and maybe have a solution?

I just printed a cube in Cura and this is a S3D slicer issue. Off to the S3D forums to post there. :slight_smile: :slight_smile: